Piston Rod

consult


Mariso is using LR approved welding procedures/materials/personnel to recondition piston rod and restore it to the original dimensions. The hardness of piston rod after heat treatment reaches 400HRB which enables the piston rod to have strong wearability.


Before reconditioning 


Final machining CNC horizontal lathe


Automatic arc-submerging welding


Magnetic particle test




Major reconditioning procedures: 


  • Pre-machining, gouging damages or cracks
  • Building up cut-off of damages or cracks by welding
  • Magnetic particle test of piston rod to verify surface defects.
  • Final machining
  • Heat Treatment
  •  Final grinding and polishing of the piston rod to standard tolerances